OIL resistant heat shrinkable tubing/oil resistant heat shrinkable tubing/oil resistant tubing/heat shrinkable tube
|
Item
|
Test Method
|
Indicator
|
|
Longitudinal length change rate
|
UL224
|
-10%~0
|
|
Tensile Strength
|
ASTM D2671
|
≥10.4MPa
|
|
Breaking Elongation
|
ASTM D2671
|
≥200%
|
|
Aging Test Of Hot Air
|
158.0ºC±1.0ºC/168h
|
-
|
|
Tensile Strength After Aging
|
ASTM D2671
|
≥7.3MPa
|
|
Elongation At Break After Aging
|
ASTM D2671
|
≥100%
|
|
Volume Resistivity
|
ASTM D876
|
≥1.0x1013Ω· cm
|
|
Withstanding Voltage
|
ASTM D2671
|
2500V,60s,Without breakdown
|
|
Water Absorption
|
ASTM D570
|
≤0.5%
|
|
Thermal shock (applicable to outer layer only)
|
-
|
225ºC,4h,No breakage, no dripping
|
|
Low-temperature resistance (applicable to outer layer only)
|
ASTM D2671
|
No breakage
|
|
Solvent Resistance (diesel lubricating oil)
|
-
|
23ºC,24h,Excellent
|