Customization: | Available |
---|---|
Certification: | ISO |
Color: | Black |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Property | Test Method | Standard Value | ||
Physical properties | Tensile Strength | ASTM-D-2671 | ≥12MPa | |
Elongation at Break | ASTM-D-2671 | ≥350% | ||
Tensile Strength after | ISO 868 | ≥10MPa | ||
Aging | ||||
Elongation at Break | ASTM-D-2671 | ≥280% | ||
after Aging | ||||
(130ºC, 168h) | ||||
Heat shock(200ºC, 4h) | UL 224 | No dripping | ||
flowing or cracking | ||||
Low temperature | ISO 974 | -40ºC | ||
flexibility | ||||
Oxygen index | ISO 4589 | ≥28 | ||
Dielectric strength | IEC 60243 | ≥20kV/mm | ||
Solvent | Gasoline | Tensile strength | ASTM-D-2671 | ≥10MPa |
resistance | Elongation at break | ASTM-D-2671 | ≥280% | |
(23ºC,24h) | Diesel oil | Tensile strength | ASTM-D-2671 | ≥10MPa |
Elongation at break | ASTM-D-2671 | ≥280% | ||
Acid & alkali | Tensile strength | ASTM-D-2671 | ≥10MPa | |
Elongation at break | ASTM-D-2671 | ≥280% |
Property | Test Method | Standard Value |
Tensile Strength | ASTM-D-638 | ≥10MPa |
Elongation at Break | ASTM-D-638 | ≥300% |
Dielectric Strength | IEC 60243 | ≥20kV/mm |
Volume Resistivity | IEC 60093 | ≥1×1013Ω·cm |