Property | Test Method | Standard Value |
Tensile Strength | ASTM-D-638 | ≥8MPa |
Elongation at Break | ASTM-D-638 | ≥300% |
Tensile Strength Variation After Heat Aging(130ºCx168h) | ASTM-D-5510 | ≤±30% |
Elongation at Break Variation After Heat Aging(130ºCx168h) | ASTM-D-5510 | ≤±30% |
Volume Resistivity | IEC 60093 | ≥1x1014Ω.cm |
Dielectric Strength | IEC 60243 | ≥20kV/mm |
Tracking Strength | IEC 60587 | 1A3.5 |
Dielectric Constant | IEC 60250 | ≤5 |
Heat Shock | 160ºC,4h | No Crack |
Water Absorption(23±2)ºC 24h | ISO 62 | ≤0.1% |
Hardness(Shore A) | ISO 868 | ≥80 |