Property | Test Method | Standard Value |
Tensile Strength | ASTM-D-638 | ≥10MPa |
Elongation at Break | ASTM-D-638 | ≥300% |
Dielectric Strength | IEC 60243 | ≥20kV/mm |
Volume Resistivity | IEC 60093 | ≥1×1013Ω·cm |
Property | Test Method | Standard Value | ||
Physical properties | Tensile Strength | ASTM-D-2671 | ≥12MPa | |
Elongation at Break | ASTM-D-2671 | ≥350% | ||
Tensile Strength after Aging |
ISO 868 | ≥10MPa | ||
Elongation at Break after Aging (130ºC, 168h) |
ASTM-D-2671 | ≥280% | ||
Heat shock(200ºC, 4h) | UL 224 |
No dripping flowing or cracking |
||
Low temperature flexibility |
ISO 974 | -40ºC | ||
Oxygen index | ISO 4589 | ≥28 | ||
Dielectric strength | IEC 60243 | ≥20kV/mm | ||
Solvent
resistance (23ºC,24h) |
Gasoline | Tensile strength | ASTM-D-2671 | ≥10MPa |
Elongation at break | ASTM-D-2671 | ≥280% | ||
Diesel oil | Tensile strength | ASTM-D-2671 | ≥10MPa | |
Elongation at break | ASTM-D-2671 | ≥280% | ||
Acid & alkali | Tensile strength | ASTM-D-2671 | ≥10MPa | |
Elongation at break | ASTM-D-2671 | ≥280% |
Product No. | L1/±5mm | L2/±3mm | D1/mm | D2/mm | ||
As Supplied |
After Recovered |
As Supplied |
After Recovered |
|||
WRSY-28/13 | 120 | 38 | ≥28 | ≤13 | ≥9 | ≤4 |
Product No. |
D1 | D2 |
L1± 10% |
L2± 10% |
L3± 10% |
δ1± 20% |
δ2δ3 ±20% |
||
As Supplied |
After Recovery |
As Supplied |
After Recovery |
||||||
C2111 | 13.5 | 6.0 | 6.6 | 3.3 | 24.0 | 15.5 | 25 | 2.0 | 1.5 |
C2121 | 27.0 | 12.4 | 13.2 | 6.1 | 53.3 | 33.3 | 55 | 2.5 | 2.0 |
Product No. |
D1 | D2,3,4 |
L± 10% |
L1± 10% |
L2± 10% |
δ± 20% |
δ± 20% |
||
As Supplied |
After Recovery |
As Supplied |
After Recovery |
||||||
C3111 | 14 | 6.6 | 6.6 | 3.6 | 46 | 15.7 | 31 | 2.0 | 1.5 |
C3121 | 27 | 13.2 | 13.2 | 6.9 | 94 | 33.0 | 57 | 2.5 | 2.0 |